Standard Designation: BPV Section VIII Div 1

Edition/Addenda:

Para./Fig./Table No:

Subject Description: Section VIII, Division 1 (1986 Edition, 1987 Addenda), UG-99

Date Issued: 12/13/1988

Record Number: BC88-363

Interpretation Number: VIII-1-89-51

Question(s) and Reply(ies): Question: A vessel has been fabricated and hydrostatically tested, and the data report
form has been signed. During preparation for shipment an arc strike is detected on the
vessel wall. The subsequent grinding to remove the arc strike reduced the vessel wall
thickness to a value below the calculated minimum. In accordance with the requirements
of Section VIII, Division 1 the vessel does not require PWHT. The thickness is restored
by welding using a qualified welder and a qualified welding procedure. The surface metal
buildup is examined in accordance with UW-42. The Inspector was notified prior to the
performance of the repair. Must the vessel be hydrostatically tested again and a new data
report form prepared and signed?
Reply: Yes.