Question(s) and Reply(ies):
Background: A weld test coupon for a PQR was welded to
itself using P-No. 1, Group 2 plate material and postweld heat
treated at 1110°F to 1130°F (600°C to 610°C) for 10 hr. The
PQR documents all supplementary essential variable notch-
toughness requirements. Notch toughness is required and all
qualification ranges are supported by the PQR for production
welds.
Reply: Yes.