Subject :SHIELDED METAL ARC WELDING ( SMAW )
Lesson Title :WELDING DEFECTS CAUSES AND REMEDIES ( UNDERCUT)
Learning Competency: LO 1. WELD CARBON STEEL PLATES IN VERTICAL POSITION (3F)
References : WELDING ON CARBON STEEL PIPES USING SMAW MODULE LAS No.: 17
CONCEPT NOTES

WELDING DEFECTS CAUSES AND REMEDIES (UNDERCUT)


CAUSES:
1. Faulty Electrode or poor manipulation
2. Faulty Electrode use
3. Correct to high
REMEDIES;
1. Use a uniform weave in butt welding
2. Avoid using an overly large electrode
3. Avoid excessive weaving
4. Use moderate current weld slowly