SA/AS-1548 2008 Identical except for steelmaking process, marking, chemical 2008
(R2018) composition, and test reports as shown in the specification.
Appendix "Interchangeability of Strength Grades" does not
apply.
SA/CSA-G40.21 2013 Identical except for marking, chemical composition, controlled 1992 and 2004 through 2013
(R2018) and normalized rolling, and test reports as shown in the (R2018)
specification.
SA/EN 10025-2 2019 Identical except for marking, chemical composition, …
resurfacing by welding, and test reports as shown in the
specification.
SA/EN 10028-2 2017 Identical except for marking, delivery condition, chemical 2003 through 2017
composition, tension test, impact test sampling, steelmaking
process, quality, and test reports as shown in the
specification. For Grade 13CrMo4-5, other acceptable
editions are limited to 2009 and later. For other acceptable
editions prior to 2017, plate thickness shall not be greater
than 250 mm.
SA/EN 10028-3 2017 Identical except for marking, chemical composition, impact 2003 through 2017
test sampling, steelmaking process, quality, and test reports
as shown in the specification. For other acceptable editions
prior to 2017, plate thickness of Grades P460NH, P460NL1,
and P460NL2, shall not be greater than 100 mm.
SA/EN 10028-4 2017 Identical except for marking, chemical composition, tension, 2003 through 2017
impact tests, steelmaking process, surface imperfections,
repair welding, and test reports as shown in the
specification.
SA/EN 10028-7 2016 Identical except for marking, heat treatment and test reports, 2000 through 2016
as shown in the specification. For the latest adopted edition,
heat treatment shall be per the Tables of Annex A; for other
acceptable editions prior to 2007, heat treatment shall be
per the Tables of Annex B. For other acceptable editions
prior to 2016, plate thickness of Grades X2CrNi12 and
X6CrNiTi12, shall not be greater than 25 mm.
SA/EN 10088-2 2014 Identical except for marking, dimensions, delivery condition, 2005 through 2014
resurfacing by welding, extent of testing, and test reports as
shown in the specification.
SA/EN 10088-3 2014 Identical except for marking, dimensions, test/inspection 2005 through 2014
documents, repair welding, heat treatment, and surface
quality as shown in the specification.
SA/EN 10216-2 2013 Identical except for marking and test reports as shown in the 2002+A2:2007 through 2013
specification.
SA/EN 10217-1 2019 Identical except for material, inspection, marking, resurfacing …
by welding, and test reports as shown in the specification.
SA/EN 10222-2 2017 Identical except for marking, resurfacing by welding, and test …
reports as shown in the specification.
SA/GB 713 2014 Identical except for chemical composition, marking, controlled …
rolling, heat treatment, and test reports as shown in the
specification.
SA/IS 2062 2011 Identical except for chemical composition, marking, …
mechanical property limits, delivery condition, repair