Professional Documents
Culture Documents
Bored Pile
Bored Pile
Procedure
Content
2. Insert casing
casing must be stand vertical
( by checking verticality of casing
when insert casing )
Bored Pile Procedure
3. Drilling
Drilling Machine :
weight : 130tons
BG - 40 drilling depth : 49m
diameter : 3m
BG - 40
weight : 96tons
BG - 28 drilling depth : 39m
diameter : 2.5m
weight : 91tons
BG - 28 SD - 515 drilling depth : 36m
diameter : 2.5m
SD - 515
Bored Pile Procedure
4. Removing slime
when finish drilling , we use Mechanical
pump equipment to remove slime .
Bored Pile Procedure
5. KODEN Test
KODEN test utilizes the principle of ultrasonic wave travel from sensor to the wall of
drilled hole and reflect to the sensor through the bentonite slurry.
Equipment
KODEN equipment consists of two parts, recorder unit and winch unit .
1. Remove any obstacle around the hole area in order that the test equipment can
access to the hole .
2. Place the winch unit over the top of drilled hole or on the steel casing.
Position the sensor (probe) at the center of the hole .
3. Lower the sensor into bentonite slurry. Hold the sensor at depth
approximately 1 to 1.5m .
4. Restore the sensor to the starting position and perform the test.
Bored Pile Procedure
Test Result
Test results are presented in graphical plot and show characteristics below :
1. Profile along two perpendicular axes.
7. Insert Tremie
Bored Pile Procedure
1m Length
2m Length
3m Length
Bored Pile Procedure
Quality of Concrete :
Max. size of Aggregate : 2.5cm
Workability : 55cm ( Flow )
Bored Pile Procedure
Strength of concrete :
► Design strength : fck =300kg/cm² ( 28day’s cure concrete )
► Strength of mix ( Target Strength ) : according to the Standard Specifications of Concrete
( Korea Concrete Institute )
Material Strength
Calculation of fck ( Mpa ) Strength of mix ( Mpa )
Target Strength 21 > fck fck + 7
( Standard specifications of concrete
)
21 ≤ fck ≤ 35 fck + 8.5
9. Remove casing
Cycle Time of a Bored Pile