BeCu Tensile Test Worksheet

All entries by Quality Manager unless noted otherwise


BeCu Foil Specimens, .006” or less thickness, BeCu Strip Specimen, more than .006” thickness,
5 ea 6” x1/2” Grain direction is lengthwise 1 ea x 9”x3/4” Grain direction is lengthwise
Matl Lot #: Thickness Matl Lot #: Thickness
Heat treat 2 hours at 615 deg F Heat treat 2 hours at 615 deg F
Furnace: Date: Furnace: Date:
Hardness Test, Knoop Scale, 5x5 readings on Hardness Test, Knoop Scale, 1x5 readings on
each specimen (don’t record tensile) each specimen (don’t record tensile)
By: Date: By: Date:
#1-1 #2-1 #1-1
#1-2 #2-2 #1-2
#1-3 #2-3 #1-3
#1-4 #2-4 #1-4
#1-5 #2-5 #1-5
#3-1 #4-1
#3-2 #4-2
#3-3 #4-3
#3-4 #4-4
#3-5 #4-5
#5-1
#5-2
#5-3
#5-4
#5-5
Translation Knoop Readings to Tensile - KSI Translation Knoop Readings to Tensile - KSI
Avg. #1 Tensile#1 Avg. #1 Tensile#1
Avg. #2 Tensile#2
Avg. #3 Tensile#3
Avg. #4 Tensile#4
Avg. #5 Tensile#5
Tensile Strength Comparison Data (KSI) Tensile Strength Comparison Data (KSI)
ASTM MTR ITM from Lab data ASTM MTR ITM from Lab data
Typical above Typical above

Review and Conclusion Review and Conclusion

Accept: Reject: Accept: Reject:


Signed: Date: NC/CAR: