Chemical Coimposition

%
C Si Mn P S Cr Mo Ni V
80crv2 .75-.85 .15-.35.30-.50 .025 .010 .40-.60 .10 .40 .15-.25
65Mn .62-.70 .17-.37.90- <=.035 <=.035 .025 .025
1.20 Max Max
75 Cr1 0.74- 0.25- 0.65- 0.025% 0.010% 0.30-
0.80% 0.45% 0.80% max max 0.45%
SK5 .80-.90 .15Max .30-.50 .030Max .030 .3 Max .025
Max

Physical Properties
65Mn 75 Cr1 80crv2 SK5
Tensile Strength 980 MPa 1000 Rolled 1300 725–970 Rolled
(680 Annealed) 460–625 Annealed
Yield Strengt 784 MPa 700 Rolled 990 450-1850
720 Annealed
Hardness 302Hb =310 (42/44HRC and -
VPN 48/50HRC) 44-48HRC