You are on page 1of 4

REKAMAN INSPEKSI TANKI BALAS

BALLAST TANK INSPECTION RECORD

Rekaman Inspeksi Tanki Balas (contoh)


Ballast Tank Inspection Record (Example)
(Refer to the company guidance provided by IACS)
1. Single Hull Tanker
Tank No. : 3 Wing Ballast Tank (P) Tank Protection1) C
Structure2) Coating Condition3) Remarks
Areas under consideration
Upper Middle Lower
Fore Transverse Bulkhead F G G
Aft Transverse Bulkhead F G G
Side Shell F F F
Longitudinal Bulkhead F G G
Deck F
Bottom F

Overall Tank Ratings FAIR To be examined at next


annual survey
Notes:
1) C: Coating, A:Anodes, NP:No Protection
2) The structure includes plating and attached structural members
3) G:Good, F:Fair and P:Poor in accordance with Table I, reproduced herein below
4) Other than “Good” condition, locations and structure members are to be reported. For instance, a case of
“Fair” condition.

2. Double Hull Tanker


Tank No. : No.1 Double Bottom Tank (P) Tank Protection 1) C, A
Coating Condition 3) Remarks 4)
Structure 2) Areas under consideration
Lower Upper
Double Bottom Tank P F

OVERALL TANK RATING POOR To be examined at next annual survey

Tank No. : No.1 Double Hull Side Tank (P) Tank Protection 1) C, A
Areas under consideration Remarks 4)
Double Hull Side Tank
Upper Middle Lower
Fore Transverse Bulkhead F G G
Aft Transverse Bulkhead F G G
Side Shell F F F
Longitudinal Bulkhead G G G
Deck G
Bottom G

OVERALL TANK RATING FAIR To be examined at next annual survey

Table I IACS clarification of “GOOD”, “FAIR” and “POOR” coating conditions


GOOD(3) FAIR POOR
Breakdown of coating or area rusted
<3% 3-20% >20%
(1)
Area of hard rust scale (1) - <10% ≥10%

JSKS-SHQE FORM-JP-06-47V(1/3)/1/2011.05. 18
REKAMAN INSPEKSI TANKI BALAS
BALLAST TANK INSPECTION RECORD

Local breakdown of coating or rust


<20% 20-50% >50%
edges or weld lines (2)
Notes
(1) % is the percentage of the area under consideration or of the “critical structural area”
(2) % is the percentage of edges or weld lines in the area under consideration or of the “critical structural
area”
(3) spot rusting i.e. rusting in spot without visible failure of coating.
(4) Other than “GOOD” condition, locations and structure members are to be reported. For instance, a
case of “FAIR” condition. “Fiar coating member:Upper deck plating Fr. No.45 to Fr.85”.

Rekaman Inspeksi Tanki Balas


Ballast Tank Inspection Record
(Dilaporkan setiap 6 bulan / Should be reported in every 6 months)

1. Single Hull Tanker (If applicable)

Tank No. : Tank Protection1)


Structure2) Coating Condition 3)
Remarks
Areas under consideration
Upper Middle Lower
Fore Transverse Bulkhead
Aft Transverse Bulkhead
Side Shell
Longitudinal Bulkhead
Deck
Bottom

Overall Tank Ratings

Photos;

JSKS-SHQE FORM-JP-06-47V(2/3)/1/2011.05. 18
REKAMAN INSPEKSI TANKI BALAS
BALLAST TANK INSPECTION RECORD

2. Double Hull Tanker (If applicable)


Tank No. : No.1 Double Bottom Tank (P) Tank Protection 1)
Coating Condition 3) Remarks 4)
Structure 2) Areas under consideration
Lower Upper
Double Bottom Tank

OVERALL TANK RATING POOR To be examined at next annual survey

Tank No. : No.1 Double Hull Side Tank (P) Tank Protection 1) C, A
Areas under consideration Remarks 4)
Double Hull Side Tank
Upper Middle Lower
Fore Transverse Bulkhead
Aft Transverse Bulkhead
Side Shell
Longitudinal Bulkhead
Deck
Bottom

OVERALL TANK RATING FAIR To be examined at next annual survey


Photos :

JSKS-SHQE FORM-JP-06-47V(3/3)/1/2011.05. 18