Professional Documents
Culture Documents
3 Coating Log
4.3.1 Primary Surface Preparation
Sheet No.:
Hull No. Inspection date
2
Plate numbers Area (m )
Name of shipyard/
steel manufacturer
Environment
Time of day Remarks
Relative humidity, %
o
Dew point, C
o
Air temperature, C
o
Steel temperature, C
Surface preparation
Method Remarks
Grain size
Surface profile, µm
Shopprimer
Manufacturer Remarks
Product name
Identification mark/number
Manufacture'
s
recommended DFT, µm
Measured DFT, µm
Curing
Jotun suggested procedure for coating inspection and repair according to PSPC, Version 2 January 2010 Page 21
4.3.2 Secondary Surface Preparation
Sheet No.:
2
Block/Tank no. Area (m )
Environment
Time of day Remarks
Relative humidity, %
o
Dew point, C
o
Air temperature, C
o
Steel temperature, C
Surface preparation
Method Remarks
Grade
Surface profile, µm
Steel condition
Sharp edges Remarks
Welding beads
Weld spatter
Other contamination
Coating inspector'
s name:
Signature:
Jotun suggested procedure for coating inspection and repair according to PSPC, Version 2 January 2010 Page 23
4.3.3 Coating Application
Sheet No.:
Hull No. Inspection date
2
Block/Tank no. Area (m )
Environment
Date
Time of day
Relative humidity, %
o
Dew point, C
o
Air temperature, C
o
Steel temperature, C
Surface condition
Coating system
Manufacturer
Product name(s)
Identification mark/number
Batch number
Date of application
Stripe coat
Jotun suggested procedure for coating inspection and repair according to PSPC, Version 2 January 2010 Page 24
Coating inspector'
s name:
Signature:
2
Block/Tank no. Area (m )
Coating
Manufacturer
Product name
Identification mark/number
Batch number
Date of application
<288
288-320
>320
Total 100%
DFT, µm Maximum
Minimum
Average
Remarks
Jotun suggested procedure for coating inspection and repair according to PSPC, Version 2 January 2010 Page 25