(As per Is 2386 (Part-1) and MORT&H Specifications )
Project- Widening of single lane to double lane from shankarampet to narayankhed
(via) regode from 1/0 to 14/0 Agency - SLMI Infra Ltd. Sample No. Date of sampling Type of material Chainage Date of testing Source material Proposed use
Wt. of agg. Wt. of agg. Ret. From
Is Sieve size (mm) Weight of agg. Wt. of agg. Ret. Passing through length gauge after ret. taken(A) (gm) On thickness thickness gauge On thickness gauge. Passing Retained gauge (B) (gm) (C) (gm) (D) (gm) 63 50 50 40 40 31.5 31.5 25 25 20 20 16 16 12.5 12.5 10 10 6.3 Total weight Remarks : Flakiness Index (F.I)= C/A x 100 = Elongation Index (E.I) = D/B x 100 = Combined FI & EI = Specification Limit (Maximum ) % =