Production Technology of EPSBR

SBR1778 Product Standard

No. Indexes Premium grade Grade I Qualified

1 Volatile, % ≤ 0.75 ≤ 1.0


2 Total ash, % ≤ 0.50 ≤ 1.0
3 Organic acid, % 3.9 ~ 5.7 3.9 ~ 6.8
4 Soap content, % ≤ 0.5
5 Bound styrene, % 22.5 ~ 24.5
6 Oil content, % 25.3 ~ 29.3 24.3 ~ 30.3
7 Mooney viscosity of raw rubber, ML1+4 100℃ 40 ~ 50 39 ~ 51 38 ~ 52
100℃
8 Mooney viscosity of M-PUR, ML1+4 ≤ 64
25min 6 ~ 10 5 ~ 10
300% tensile stress at a
9 given elongation (145 ℃ ), 35min 10 ~ 14 9 ~ 14 9 ~ 14
MPa
50min 12 ~ 16 11 ~ 16
100℃
10 Mooney viscosity of M-PUR, ML1+4 ≥ 17.5 ≥ 16.5
100℃
11 Mooney viscosity of M-PUR, ML1+4 ≥ 430 ≥ 410