X1
X2
X3
X4
X5
X6
X7
X8
X9
X10
JAWABAN
X1 No Defect
X2 Elongated Cavity
X3 Distributed Porosity
X4 Clustered Porosity
X5 Linear Porosity
X6 Linear Slag Inclusion
X7 Continuous Undercut
X8 Incomplete Penetration
X9 Worm Hole
X10 Root Fusion