Plate Thumb Print Report Example

Name (Block capitals) Joe BLOGGS Signature Joe Bloggs Test piece identification Example 1

Code used BW/VI/00 Welding process MMA (SMAW) Joint type Single V Butt

Welding position Flat 1G/PA Length & thickness L=300mm t = 12.5mm Date 16/07/0

A B C

Note: all dimensions in mm


Plate Sample Cap
Welding Process MMA (SMAW)

Slag Cap Undercut 100 Lack of Cap Undercut


sidewall fusion Intermittent
5 Inclusion 25 Intermittent 160 L= 15 ,D= 1.0 max
L= 10,W=4 L= 15 ,D= 1.0 max L= 10

Cap Undercut Cluster


Intermittent 50 Porosity
15 L= 30,D= 1.6 L=5 w = 3 200 Arc Strike 10

15

•Note: All dimension in mm


Spatter and surface slag requires removal, arc strikes require grind smooth and check with MT
Poor cap profile full weld length
Linear misalignment full weld length D = 1.0 max
Final Report

After you have completed your thumb print report sketch of


your test plate the next step is to complete your final report
again the report must be completed in ink (no pencil).

The report must be completed to your thumb print sketch,


do not leave any boxes empty, every box must be
completed or dashed out. You must also make any
comments you feel are necessary regarding any defects
observed.

The report form used in CSWIP will look like the following
example.
Print full name : Joe Bloggs

Plate identification : Example 1

Defect type Pipe/plate Accumulative Maximum Accept/Reject


section no Total Table

Reinforcement (Height) A-C L= 10 , D = 3.0 2.0 Rejected


Reinforcement (App)
Incomplete filling
Inadequate weld width
Slag inclusions
Undercut
Surface porosity
Cracks
Lack of fusion
Arc strikes
Mechanical damage
Laps/Laminations
Misalignment