Professional Documents
Culture Documents
Fosroc Brushbond TGP: (Formerly Tegraproof C)
Fosroc Brushbond TGP: (Formerly Tegraproof C)
(Formerly Tegraproof C)
Sewage treatment and water treatment plants Following stripping of formwork, water jet or acid etch as
Water tanks above to remove all traces of form oil and surface laitance.
Remove all debris from the work area before proceeding
Concrete pipes
with thorough saturation (with clean potable water) of the
Manholes area prior to the next stage of the works.
Advantages Mixing
Surface damage will not affect the system Do not mix more material than can be safely used in 20
minutes at 25°C @ 50% RH. If the mixture thickens, re-stir to
Description reduce consistency, do not add water.
Old concrete
water jetting.
Fosroc Brushbond TGP
Slurry coat for existing concrete Technical support
Brushbond TGP slurry coat can be applied with a soft brush, Fosroc offers a comprehensive technical support service to
broom, or plaster sprayer. Ensure the slurry is worked well specifiers, end users and contractors. It is also able to offer
into openings, rough surfaces, joints and routed out areas. on-site technical assistance, an AutoCAD facility and
Make the second application when the first coat has reached dedicated specification assistance in locations all over the
initial set (usually within one hour dependent upon world.
temperature). If the first coat has dried out, moisten the surface
prior to applying the second coat. Estimating
Active water leaks should be pre-sealed by using a rapid Supply
setting plugging mortar Renderoc Plug (see separate data Brushbond TGP : 20 kg bags
sheet), prior to application of Brushbond TGP.
Coverage
Curing and protection Brushbond TGP : 1 to 1.5 kg/m2 per application (brush)
Brushbond TGP applications must be kept moist for a 1.2 to 1.3 kg/m2 per application (dry
minimum of 48 hours therefore following initial set, curing by shake)
water spraying is recommended. The treated surface shall Actual coverage rates will depend upon the profile and porosity
be ‘fog’ sprayed a minimum of 3 to 4 times daily for the 48 of the substrate.
hour period.
Head Office
telephone: (+9714) 2039699 fax: (+9714) 2859649 email: agf@fosroc.com
Al Gurg Fosroc LLC
Regional offices
Post Box 657, Dubai Abu Dhabi, Al Gurg Fosroc telephone: 673 1779 fax: 673 1449 email: abudhabi@fosroc.com
United Arab Emirates Bahrain, YBA Kanoo telephone: 17738200 fax: 17732828 email: bahrain@fosroc.com
Kuwait, Boodai telephone: 4817618 fax: 4832124 email: kuwait@fosroc.com
www.fosroc.com
Oman, Al Amana telephone: 24815080 fax: 24817554 email: oman@fosroc.com
Qatar, Tadmur telephone: 4432365 fax: 4419517 email: qatar@fosroc.com
UAE/0245/10/H