You are on page 1of 1

THANBEE PRINT WORLD LTD.

PRINT DURABILITY TEST REPORT

Buyer Name: — VF-The North Face Received Date: — 27/01/2024

Order/Style No: — A89EJ+A89EV Reporting Date: — 28/01/2024

Body Color: — Olive Testing Stage: — Sample

Print Type: — Rubber Print Sample Type: — Strike off

Print Color: — Applicant’s: — Mr. Alim

Fabric Type: — Fleece Others: —

Report No: — VFN~SAM0498-0124A

TEST CONDUCTED

PRINT DURABILITY TEST—Appearance after washing/drying:

VFOI-004/AATCC 135 (Domestic washing)


(Machine wash at 40°C, Followed By Line Dry)
AATCC 1993 Standard Reference Detergent (WOB) 20g/wash, Using Miele, Wash inside out.

Observation After 01st Washing After 05th Washing After 10th Washing Requirement

Colour Change of Fabric 4-5 4-5 4-5

Colour Change of Print 4-5 4 4

Cracking No Cracking Observed No Cracking Observed No Cracking Observed


Class 4.0
Change of Surface Negligible Negligible Negligible

Appearance of Print Found Okay Found Okay Found Okay

Comments: After 01st, 05th, 10th time washes the overall print durability found as acceptable.

Final Result: Accepted √ Rejected

N.B.: This report is only for internal reference.

Prepared by Checked by
THANBEE PRINT INHOUSE LAB
Sardagonj, Kashimpur, Gazipur.