DEFECT CATEGORY IDENTIFICATION AND TREATMENT METHOD

ITEM CATEGORY CLASSIFICATION ILLUSTRATION TREATMENT METHOD MATERAIL

- STEP 1: CHIPPING OF DEFECTIVE OR DETERIORATED CONCRETE TO REACH


QUALIFIED CONCRETE
COLUMN AND WALL - STEP 2: REMOVE ALL RUST FROM REINFORCEMENT AND MAKE ROUGHING NORMAL CONCRETE CONTRACTOR :

BIG HONEYCOMB CONCRETE SURFACE WITH HIGH SLUMP


NOT FULL FILL OF CONCRETE
- STEP 3: WASH AND CLEAN THE ENTIRE SURFACE BEFORE TAKING UP & CONCRETE STRENGTH 50MPa
REPAIRS
- STEP 4: CASTING NORMAL CONCRETE WITH HIGH SLUMP, HIGHER
STRENGTH (C50) & LAYING SIKALATEX BEFORE POURING CONCRETE

HONEYCOMB CONCRETE

- STEP 1: CHIPPING OF DEFECTIVE OR DETERIORATED CONCRETE TO REACH


QUALIFIED CONCRETE
- STEP 2: REMOVE ALL RUST FROM REINFORCEMENT AND MAKE ROUGHING SIKA LATEX MORTAR
SMALL HONEYCOMB CONCRETE DEFECTED SURFACE SURFACE
- STEP 3: WASH AND CLEAN THE ENTIRE SURFACE BEFORE TAKING UP
REPAIRS
- STEP 4: APPLY SIKA LATEX MORTAR

FOR CONSTRUCTION

NOTE: CANA SINO CONSTRUCTION CORPORATION - CSCC

SIKA LATEX MORTAR RATIO: CEMENT : SAND : LIQUID (1 PART SIKA LATEX + 1 PART WATER) = 1.5 : 2 : 1 DRAWN BY: MR. MAK BUNLEANG

CHECKED BY : MR. HEAT AREY

APPROVED BY : MR. VO VAN LUC

MEGA ASSET MANAGEMENT

CHECKED BY : MR. KHU0Y VANNTEX


MR. LEU YIMBAC

APPROVED BY : MR. UNG MENGHONG

OCIC- TECHNICAL TEAM

CHECKED BY : MR. HEANG KIMHAK

MR. LONG CHANRADY

APPROVED BY : MR. TAN LIP JIN

DRAWING TITLE:

BUILDING-E CONCRETE REPAIRING METHOD

DRAWING No: MOS-RV-01


DATE: 10-08-2020

REV: 00

You might also like