You are on page 1of 4

GEO-CHEM LABORATORIES PVT . LTD.

Plot No. 306, Udyog Vihar, Phase-2


Gurgaon, Haryana - 122016. India.
TEL.: + 0124 6250500
Email: qa.c p@geoc hem-cp.c om
CIN: U74220MH1964PTC01 3022
International
Independent Inspection
&
Testing Company
TEST REPORT
Report No.: GCGNTX2218636 Dated: 17 Aug 2022
ULR No. TC637122000007657F
Applicant : Loop
Contact Person : Mr. Rishab Kedia
Address : 107/A/2, G.T. Road Howrah-711106

Sample not drawn by Geo-Chem Laboratories Pvt. Ltd.


Sample Description : Submitted Sample are Knitted garments
Color : Grey Melange & SINKAR 114
Style no. : DPAW22BNP4
Buyer : First Cry
Brand : Doodle Poodle
Buyer Contact : Not Provided
Submitted Fibre Content : 70% Cotton, 30% Polyester &100% Cotton (On TRF)
Article No. : DPAW22BNP4
Order No. : Not Provided
Age Group : 0-4 Y (On TRF)
Test Package Name : Knit Garment- (Washable)
:
End Use Not Provided
Country of Destination : Not Provided
Sample Received Date : 17 Aug 2022
Testing Period : 14 Aug 2022 to 17 Aug 2022
Aapplicant Care Instruction :

Wash inside out, machine wash cold, mild cycle wash with like colors only,
only non-chlorine bleach when needed, dry clean if needed, cool iron, flat dry,
do not wring, iron on reverse.
S. No. Test Conducted Tested Component Results
1 Dimensional Stability to Washing (1st Wash) Top & Bottom P
2 Color Fastness to Washing Top & Bottom P
3 Color Fastness to Rubbing Top & Bottom P
4 Fibre Composition Top & Bottom P
5 Fabric Weight Top Refer Result
6 Seam Bursting Strength Top & Bottom P
7 Spirality After Washing Top P
Bottom NA
8 Color Fastness to Perspiration Top & Bottom P
P=Pass, F=Fail, NA: Not-Applicable.
For and on behalf of
Geo-Chem Laboratories Pvt. Ltd.

Nitin Jangra
Asst. Manager
Authorized Signatory
Remark:
1. The sample were conditioned and tested in environmental conditions Temperature 20°C (±2) and relative humidity 65% (±4).
2. Statement of conformity and decision rule will be given (if applicable).
Test result is drawn according to the kind and extent tests performed.
Without permission of the tests center, this report is not permitted to be duplicated in extracts. This report does not entitle to carry any safety mark on this or similar
products. This test report represents the test parameters as requested by the customer based on submitted sample only

Regd. Off.: Geo-Chem House, 294, Shahid Bhagat Singh Road, Fort, Mumbai 400001. India.
www.geochem.net. in
Page 1 of 4
Report No.: GCGNTX2218636 Dated: 17 Aug 2022

RESULTS
1. DIMENSIONAL STABILITY AFTER WASHING (AFTER 1ST WASH)
Test Method: ISO 6330: 2012
Washing Procedure: Wash Inside Out, Wascator Washing Machine Front Loading Horizontal Drum type, Test No. 3M at 30° With 2
kg Load in Detergent solution followed by Flat Dry.
RESULT (Top)
Dimensional Change Requirement
Measuring Position Original After 1st Wash
After 1st Wash (%)
Shoulder 21.0 20.5 -2.4
Chest 25.5 24.9 -2.3
Armhole 10.6 10.3 -2.8
Bottom 25.7 25.0 -2.7 Length & Width: ±5%
Centre Back Length 32.3 30.5 -5.0
Sleeve Length 10.0 9.4 -5.0
Side seam 22.6 21.3 -5.0
HSP 35.0 33.0 -5.0

RESULT (Bottom)
Dimensional Change Requirement
Measuring Position Original After 1st Wash
After 1st Wash (%)
Waist Relaxed 18.0 17.5 -2.8
Front Rise Seam 15.0 14.2 -5.0
Back Rise Seam 18.5 17.5 -5.0 Length & Width: ±5%
Hip 26.0 25.3 -2.7
Leg Opening 13.6 13.3 -2.2
Total Length 22.2 21.0 -5.0

2. COLOR FASTNESS TO WASHING


ISO 105 C06:2010
Test No. A2S, TEST 30 MIN MECHANICAL WASH AT 40°C IN DETERGENT SOLUTION WITH 10 STEEL BALLS
RESULT (GRADE) Requirement
Top
Color Change 4 All 4
Color Staining on Acetate 4-5
Color Staining on Cotton 4-5
Color Staining on Nylon 4-5
3-4
Color Staining on Polyester 4-5
Color Staining on Acrylic 4-5
Color Staining on Wool 4-5
Self-staining 4-5 4-5

3. COLOR FASTNESS TO RUBBING


ISO 105 X 12:2016
RESULT (GRADE) Requirement
Top Bottom
Dry 4-5 4-5 3-4
Wet 4 4 3

Regd. Off.: Geo-Chem House, 294, Shahid Bhagat Singh Road, Fort, Mumbai 400001 . India.
www.geochem.net. in

Page 2 of 4
Report No.: GCGNTX2218636 Dated: 17 Aug 2022

4. FIBRE COMPOSITION
ISO 1833-1
RESULT (Top) Claimed

FIBRE COMPOSITION Lab Analysis


(On Garment Basis) 70% Cotton 30% 70% Cotton
Polyester 30% Polyester
(No Tolerance for
Single fiber,
±3.0% Tolerance for
FIBRE COMPOSITION Recommended Blend fibers)
(On Garment Basis) 70% Cotton 30%
Polyester

RESULT (Bottom) Claimed

FIBRE COMPOSITION Lab Analysis


100% Cotton
(On Garment Basis) 100% Cotton
(No Tolerance for
Single fiber,
±3.0% Tolerance for
FIBRE COMPOSITION Recommended Blend fibers)
(On Garment Basis) 100% Cotton

5. FABRIC WEIGHT
ISO 3801
RESULT Requirement
Top
Weight (GSM) 185.5 g/m2 ±5% (As Claimed)

6. SEAM BURSTING STRENGTH


ISO 13938-1: 1999
Direction RESULT (PSI) – Top Requirement
Side Seam 63 FRS
Sleeve seam 68 FRS
50 PSI
Shoulder 52 STB
Armhole 80 FRS
FRS: Fabric Rupture at Seam, STB: Sewing thread breakdown.

Direction RESULT (PSI) – Bottom Requirement


Inside 90 FRS
Front rise 88 FRS 50 PSI
Back rise 94 FRS
FRS: Fabric Rupture at Seam.

7. SPIRALITY AFTER WASHING


ISO 16322-2: 2005
Washing Procedure: Wash Inside Out, Wascator Washing Machine Front Loading Horizontal Drum type, Test No. 3M at 30° With 2
kg Load in Detergent solution followed by Flat Dry.
RESULT Requirement
Top Bottom
Spirality (%) 4.7% NA Max. 5%

Regd. Off.: Geo-Chem House, 294, Shahid Bhagat Singh Road, Fort, Mumbai 400001 . India.
www.geochem.net. in

Page 3 of 4
Report No.: GCGNTX2218636 Dated: 17 Aug 2022

8. COLOR FASTNESS TO PERSPIRATION


ISO 105 E04:2013
RESULT (GRADE) Requirement
Acidic Alkane
Color Change 4 (All) 4 (All) 4
Color Staining on Acetate 4-5 4-5
Color Staining on Cotton 4-5 4-5
Color Staining on Nylon 4-5 4-5
3-4
Color Staining on Polyester 4-5 4-5
Color Staining on Acrylic 4-5 4-5
Color Staining on Wool 4-5 4-5
Self-Staining 4-5 4-5 4-5

COLORFASTNESS RATING COLORFASTNESS RATING


COLOR CHANGE COLOR STAIN / SELF STAINING
5 NEGLIGIBLE OR NO CHANGE 5 NEGLIGIBLE OR NO STAINING
4 SLIGHTLY CHANGED 4 SLIGHTLY STAINED
3 NOTICEABLY CHANGED 3 NOTICEABLY STAINED
2 CONSIDERABLY/DISTINCT CHANGED 2 CONSIDERABLY/ DISTINCT STAINED
1 MUCH/SEVERE CHANGED 1 HEAVILY/SEVERE STAINED

Sample Photo
End of the Test Report

Regd. Off.: Geo-Chem House, 294, Shahid Bhagat Singh Road, Fort, Mumbai 400001 . India.
www.geochem.net. in

Page 4 of 4

You might also like