On the peeled rubber, a depth measurement is carried
out, then inject the adhesive into the rubber that was
1. The end of the lagging is peeling off √
measured earlier until the peeled rubber returns to its
original state
Clean the shaft where there is corrosion using a brush
until it is clean, then clean the former brush using a
2. The shaft is not lubricated √
cleaner and continue with applying lubricant or grease
to the shaft
Clean the paint by sanding the surface that feels bad
until it is smooth, then cleaning it with a clean cloth
3. Finishing Painting is not good enough. √
before repainting until the desired specifications are met
(paint thickness).
for an uneven shaft surface, the machining process is
4. Finishing shaft is not good enough (rough) √
carried out again to get maximum results
Filler is added to the shaft that has defects according to
5. There is a hole in the shaft √
the shaft repair procedure that we have