You are on page 1of 8

Building Practice Table 1 (reference L13J Series atlas)

Applicabl
classify number name Construction practices remarks
e room
1, reinforced concrete structure self-waterproof,
Reinforced impermeability grade P6
concrete self- 2,50 thick C20 fine stone concrete protective layer;
Waterproof grade:
waterproofing 3. Isolation layer: one layer of non-woven fabric (200g /
Grade 1
basebo bottom plate + m2) Basement
combustion
ard coil 4, waterproof layer: double layer 4 + 3 thick SBS modified floor
the performance grade
waterproofing asphalt waterproof coil (type II)
earth is: Grade A
(from top to 5,100 thick polymer cement concrete, with leveling
Under
bottom) 6, plain filling soil layered compaction, compaction
room
coefficient of 94%.
outside
Side wall waterproof (anti 2):
provide
Reinforced 1,2:8 gray soil, layered compaction;
against
concrete self- 2,50 thick extruded polystyrene board protective layer, Waterproof grade:
water
exteri waterproof with polyvinyl acetate adhesive paste; Basement Grade 1
or exterior wall + 3,20 thick 1:2.5 cement mortar leveling layer exterior combustion
wall coil waterproof 4, waterproof layer: double layer 4 + 3 thick SBS modified wall performance grade
(from outside asphalt waterproof coil (type II) is: Grade A
to inside) 5, reinforced concrete structure self-waterproof,
impermeability grade P6, surface filling and dressing);
the 1. M40 emery surface layer (5 KG per square meter)
earth's 2.200-thick C25 reinforced concrete (with ^ 18@200 two-way
surface single-layer welded steel mesh);
Concrete
The 3,50 thick C20 coagulation protective layer Combustion
moisture-proof factory
ground 4,0.4 thick polyethylene film moisture-proof layer; performance grade
ground (from building
1 5,300mm thick weathered sand (mixed with 6% cement) is: A grade
top to bottom)
compaction, compaction coefficient of 0.94;
6, plain soil layered compaction leveling, compaction
coefficient of 0.94;
The Cement mortar 1,20 thick 1:2 cement mortar plaster compaction and Circulati Combustion
ground waterproof polishing; ng water performance grade
2 floor (from top 2,15 thick 1:3 fiber cement mortar bottom (mixed with Du pool, is: A grade
to bottom) Lala fiber 0.9 kg/m3 mortar); fire
3, cement-based permeable crystalline waterproof coating water
1.0 thick (dosage is not less than 1.5 kg / square meter); pump room
4,30 thick C25 fine stone concrete with tamping with ground
polishing 1.0% to find the slope to the suction well /
drainage ditch;
5, plain cement slurry together;
6, self-waterproof reinforced concrete floor
(impermeability grade is P6);
1,10 thick ground brick (reserved for secondary
decoration);
3,40 thick 1:3 dry hard cement mortar combined layer
Factory
(reserved for secondary decoration); Combustion
hall,
Face rick 4,60 thick C20 fine stone concrete (with two-way ^ 16 performance grade
The office
brick-proof spacing 200 steel mesh, surface sprinkle 1:1 cement sand is: grade A
ground area,
ground (top to with the leveling); basement roof
3 dressing
bottom) 5,0.4 thick polyethylene film moisture-proof layer; area is only 1,2
room,
6,300mm thick weathered sand (mixed with 6% cement) process
guard
compaction, compaction coefficient of 0.94;
7, plain soil layered compaction leveling, compaction
coefficient of 0.94;

1.8-10 thick anti-skid ground brick, scraping cement mortar


paste on the back of the board, thin cement mortar rubbing
seam (reserved for secondary decoration)
2.20 thick 1:3 dry hard cement mortar binding layer;
(reserved for secondary decoration)
3, the thinnest place 20 thick 1:3 cement mortar to the
Combustion
ground drain slope 1%%%
Anti-skid Toilet, performance grade
4.1.5 thick JS waterproof coating layer, brush three times,
ground brick tea room, is: A class meal
Ground brush to 300mm above the building completion surface
waterproof meal preparation room
4 (cleaning room to 1.8m high);
floor (from top preparati structure
5,20-thick cement mortar leveling layer;
to bottom) on room lowering plate
6,60 thick C20 fine stone concrete (with two-way ^ 16
300
spacing 200 steel mesh, surface sprinkle 1:1 cement sand
with the leveling);
7,0.4 thick polyethylene film moisture-proof layer;
8,300mm thick weathered sand (mixed with 6% cement)
compaction, compaction coefficient of 0.94;
9, plain soil layered compaction leveling, compaction
coefficient of 0.94;
Ground Cement mortar 1, no fire and wear-resistant hardening agent; Distribut Combustion
5 moisture-proof 2,60 thick C20 fine stone concrete (with two-way ^ 16 ion room, performance grade
ground (from spacing 200 steel mesh, surface sprinkle 1:1 cement sand power is: A grade
top to bottom) with the leveling); distribut
3,30 thick C20 coagulation protective layer ion room
4,0.7 thick polyethylene polypropylene waterproof coil;
5,60 thick C20 concrete cushion
6,300mm thick weathered sand (mixed with 6% cement)
compaction, compaction coefficient of 0.94;
7, plain soil layered compaction leveling, compaction
coefficient of 0.94;
a 1. M40 emery surface layer (5 KG per square meter);
Combustion
storied Floor Emery abrfloor 2,50 thick C20 fine stone concrete (with two-way ^ 16 factory
performance grade
building 1 (top to bottom) spacing 200 steel mesh); building
is: A grade
Face 3, cast-in-place reinforced concrete stairs
1,10 thick ground bricks, thin cement mortar rubbing seam Productio
(reserved for secondary decoration); n
2,40 thick 1:3 dry hard cement mortar (reserved for workshop
secondary decoration); in 1 # Combustion
Floor Floor floor
workshop performance grade
2 (top to bottom)
(includin is: A grade
3, cast-in-place reinforced concrete stairs g
stairwell
)
1.8-10 thick anti-skid ground brick, scraping cement mortar
paste on the back of the board, thin cement mortar rubbing
seam (reserved for secondary decoration)
2.20 thick 1:3 dry hard cement mortar binding layer;
Anti-skid (reserved for secondary decoration) Toilet,
ground brick 3, the thinnest place 20 thick 1:3 cement mortar to the tea room, Combustion
Floor
waterproof floor drain slope 1% meal performance grade
3
floor (from top 4,1.5 thick polyurethane waterproof coating layer, paint preparati is: A grade
to bottom) three times, brush to 300mm above the building completion on room
surface (cleaning room to 1.8m high);
5,20-thick cement mortar leveling layer;
6, reinforced concrete floor, surface partial repair and
leveling;
Floor Fine stone 1,20 thick 1:2 cement mortar wipe flat pressure light; High Combustion
4 concrete 2, the thinnest place of 30 thick fine stone concrete slope water performance grade
waterproof finding 1%; tank is: A grade
floor (from top 3.1.5 thick JS waterproof coating, when the wall turns over
to bottom) to the height of flooding, covered by the inner wall
plastering layer;
4, plain cement slurry together;
5, the structure of the floor with the dozen with the wipe
flat;
Cement mortar 1,20-thick cement mortar wipe flat pressure light; power Combustion
Floor
floor (from top 2, plain cement slurry together; distribut performance grade
5
to bottom) 3, reinforced concrete floor plate; ion room is: A grade
1, reinforced concrete floor plate; Dining
Aluminum buckle preparati Combustion
Ceilin
ceiling (top to 2, light steel keel supporting aluminum buckle plate on room, performance grade
g 1
bottom) ceiling (decoration reservation); tea room, is: A grade
toilet
Light steel
keel gypsum 1, reinforced concrete floor plate; Combustion
Ceilin manufactu
board suspended 2, light steel keel gypsum board ceiling (decoration performance grade
platfond g 2 ring shop
ceiling (from reservation); is: A grade
top to bottom)
1, reinforced concrete floor plate; Ceiling
2, polymer cement mortar joint filling; of other
Coated ceiling Combustion
Ceilin 3,2-3 thick flexible water-resistant putty; areas
(from top to performance grade
g 3 (includin
bottom) is: A grade
4, spray mildew-proof latex paint; g stair
floor)
1, brush the special interface agent once; All
2,12 thick 1:3 cement mortar; floors
Combustion
Cement mortar with
Kick performance
kicking (from cement
foot 1 grade: Class A
out to inside) 3,6 thick 1:2 cement mortar plaster pressing light; mortar
height 200mm
(excludin
g pool)
1.8~10 thick finished granite kicking, cement mortar seam
skirt All floor
rubbing or seam filling agent seam filling (decoration
floors
reservation);
floor
Granite kick 2,3~4 thick 1:1 cement mortar with water weight 20% Combustion
Kick tile
(from out to construction glue (or supporting professional adhesive) performance grade
foot 2 areas
inside) bonding layer (decoration reservation); is: A grade
(excludin
3, plain cement slurry together (with professional adhesive
g toilet,
paste without this process) (decoration reservation);
bathroom)
4,20-thick cement and lime mixed mortar;
interior The Face brick 1.5 Thick brick, filling material; (decoration reservation) Toilet, Combustion
wall inner waterproof 2.3 Thick ceramic tile adhesive, knead and squeeze solid; shower performance grade
wall 1 inner wall (reserved for decoration) room, is: A grade
(from outside 3.6 thick 1:2.5 cement mortar layer leveling (middle drying
to inside) pressure into a hot dip galvanized steel wire mesh, room
expansion bolt fixed) surface fine hair, 50mm putty turning kitchen,
around the door;
4.1.5 Thick polyurethane (two components) waterproof
material, brush three times, surface sand;
5.9 Thick 1:3 cement mortar bottom compaction;
dining
6. Base wall (special repair materials to repair the wall
room
gap, the surface spray interface agent, different materials
wall connection nail wire mesh, width 300);
1, reinforced concrete structure self-waterproof,
Waterproof impermeability grade P6; Inside
The Combustion
interior wall 2, cement-based permeable crystalline waterproof coating walls and
inner performance grade
(from outside 1.0 thick (dosage is not less than 1.5 kg / square meter); roof of
wall 2 is: A grade
to inside) 3,20 thick waterproof mortar three times, surface fire pool
compaction;
1,2-3 times flexible water-resistant putty batch scraping, Except
smooth, anti-proof latex paint two to three times; for the
Eatex paint
The 2,6 thick 1:0.5:3 cement lime mortar leveling (pressed into other Combustion
interior wall
inner the full hanging alkali resistant grid cloth); interior performance grade
(from out to
wall 3 3,9 thick 1:1:6 cement lime mortar walls in is: A grade
inside)
4, brush the special interface agent once; the above
5, the base level wall; area
exterior 1, the base level wall;
wall 2,2 thick equipped with a special interface agent once;
3,9 thick 2:1:8 cement mortar leveling layer;
4,6 thick 1:2.5 cement mortar;
Plant
Exteri Coated exterior 5,5 thick dry powder polymer cement waterproof mortar, the Combustion
1.5m high
or wall (from middle pressure into a layer of alkali resistant glass performance grade
brick
wall 1 inside to out) fiber mesh cloth; is: A grade
sill wall
6, moisture-proof primer, scraping flexible water-resistant
putty;
7, spray or roll to brush the bottom coating again;
8, spray or roll brush surface coating two times;
Exteri Coaint 1, the base level wall; Office Combustion
or insulation 2, brush the interface mortar together; part of performance grade
wall 2 (from inside to 3,15 thick 1:3 cement mortar leveling; the is: A grade
out) 4, paste 100 thick B1 grade polystyrene board insulation exterior
layer, supporting adhesive paste, auxiliary anchor bolt wall
fixed;
5,5 thick dry powder polymer cement waterproof mortar, the
middle pressure into a layer of alkali resistant glass
fiber mesh cloth;
6, moisture-proof primer, scraping flexible water-resistant
putty;
7, spray or roll to brush the bottom coating again;
8, spray or roll brush surface coating two times;
1, galvanized cold-bent steel beam;
Extern Pressure steel 2.0.4 thick pressed steel plate inner wall plate; Factory Combustion
al plate exterior 3,100-thick glass silk cotton felt; exterior performance grade
wall 3 wall 4. Purlin; wall is: A grade
5.0.6 thick pressed steel plate external wall plate;
1,40 thick C20 fine stone concrete (with Φ 4@150 steel
mesh) 6 mx 6 m grid, seam width 20, sealant seam;
2, the isolation layer (dry spread glass fiber cloth or low
strength grade mortar) one; Roofing
3,3 + 3 thick SBS modified asphalt waterproof coil; other Combustion
Roofin Fine stone
4,30 thick C20 fine stone concrete leveling layer; than the performance grade
g 1 concrete roof
5,100 thick extruded polystyrene board insulation layer; workshop is: A grade
6,20 thick 1:2.5 cement mortar leveling layer; roof
roofing 7, the thinnest place 20 thick 1:8 cement perlite slope
finding layer 2%%%;
8. Cast-in-place concrete floor slab;
1, 0.6mm Thick aluminum magnesium manganese pressure type
steel plate YX 51-380-760 type;
Combustion
Roofin Color steel 2,75-thick glass wool rolling felt; Factory
performance grade
g 2 plate roof 3, ≥0.17mm High-density anti-adhesive polyethylene film; roof
is: A grade
4, hot-dip galvanized or stainless steel wire mesh;
5, cold-bent steel purlin;
1,200 thick C30 reinforced concrete (with ^ 18@200 two-way
single-layer welded steel mesh);
reinforced Outdoor
Outdoor 2,300mm thick 5%~6% cement stabilized sand, divided into
Road 1 concrete factory
road two layers of rolling, compaction coefficient of 0.94;
pavement road
3, plain soil rolling, the compaction coefficient is not
less than 94%;

The steel structure node practice adopts the atlas


Practice-Choose the Practice-Choose
Node site Node site
atlas the atlas
Lverse lap of The wall is vertically
17J925-1, p. 2-7 17J925-1, p. 3-5
roof panel arranged
Drainage outer 17, J 925-1, Page 17J925-1, Page 3-
Corner-Yangjiao
eaves ditch 2-25, Node 2 19, Node 3
Drainage inner 17J925-1, Page 2- 17J925-1 Page 3-
Corner-Yin Angle
eaves ditch 26, Node 3 20 Node 4
17J925-1 Page 2-42
gutter Push pull outside the door 17J925-1 p. 3-27
Node 13
17J925-1, Page 2- 17J925-1, Page 3-
Roof cover plate In the column
27, Node 5 15, Node 2
17J925-1 Page 2-76 Roof maintenance of the steel
plane skylight 17J925-1 p. 2-61
Node 6 climbing ladder
Parapet-gable 17J925-1 Page 2-30 17J925-1 Page 3-
Window node
edge closure Node 1,2 16 Node 5,11
High and low 17J925-1 Page 2-32
flow-off 17J925-1 p. 2-60
across Node 16,17
17J925-1 Page 3-
awning 17J925-1 p. 3-32 Metope deformation seam
16 Node 7
Roofing
17J925-1 Page 2-42
deformation
Node 15
joint
Note: No paint the installation weld. The main component adopts shot blasting and rust
removal, the rust removal grade is Sa, paint two anti-rust primer after processing, paint
paint after installation, bolt connection surface, roof and wall lighting belt technical
requirements:
1. Light transmittance:> 50%, color: colorless.
2. Thickness selection: 1.5mm and above (should meet the requirements of snow load and
wind pressure of 1.5m span purlin spacing in Qingdao area)
3. Double light board: heat insulation, heat insulation and condensation prevention. The
YX 820 light panel should be the same as the glass shape of the color steel plate.
4. lap with the color steel tile: the light board should be placed on the color steel
plate.
5. For other nodes, see atlas 17J925-1.