METHOD STATEMENT FOR BRICK BAT HARDCORE


INTRODUCTION

This document desc ribes the Work Methodology to Carryout BrickBatwork in MetrodeckareaatNorthDelhiMetroMall Project, New Delhi in
a Planned & Controlled Manner with Reference to the Product Specification, Standards and Drawings .

1. MATERIALS

The following Materials or its Equivalent to be used for water proofing:

a. OPC-43 Grade & Sand confirming to IS


b. Brick Bat.

3. RESPONSIBILITIES

A) SITE INCHARGE - Shall Report to Project Manager shall be Responsible for Control, Supervision & Direction
for Implementation of this Procedure.
B) SITE ENGINEER – Shall report to Site In-Charge; shall carry out the work as per the Drawing & Specification and
make sure all the required Tests & Checks are done.
C) QA/QC ENGINEER Shall Report to QA/QC In-charge; QC Engineer shall Assist in Carrying out
Field/Lab Test; shall conduct Audit/Observation of the work done and Inform Site Engineer about the Non-
Compliances when Found.

4. WORK METHODOLOGY

 EQUIPMENTS / TOOLS

Mainly the following Tools & Equipment to be used as per Requirements while working:
o Trowel
o Mortar Pan
o Wire Brush
o Air Blower
o Chisel
o Hammer
o Pan/Tray for keeping mortar
o Water Drums/Containers
o Other Small Tools as per Requirements for convenience

5. QUALITY ASSURANCE/CONTROL

 MATERIALS
o MTC to be issued before work has started.
o Product Information Sheet is to be attached .
o Any Improvement in Methodology shall be reviewed.
STATEMENT Ref. NO.- 08
REV:- 00 DATE :- 14.02.2022
NAME: Method Statement of Brick Bat Hardcore
NDMMPL PROJECT :- DELHI 7

CONTRACTOR :- Society of Green Makers (P) Ltd. CMC :- CBRE South Asia CLIENT :- NDMMPL

6. SAFETY

 The Area where Brick bat hardcore work to be undertaken must be cordoned" and clearly sign posted to establish a
restricted area
 Other Safety A rrangements-As per Submitted Safety Plan.
 All Personnel to be fully adhered to PPE’s.

STEPWISE PROCEDURE TO CARRY BRICKBAT WORK

 Surface will be cleaned thoroughly with wire brush.

 Old loose concrete / mortar, set slurry, nails, bitumen, oils and grease to be removed properly.

 Providing the top level of the hardcore with proper marking on the spots and same will be showed to PMC in charge.

 Preparing the surface with binding material (cement mortar) 1:4 ratio.

 Fix the sized bricks as per the required levels it may varies 63mm to 90mm (Average 75mm)
STATEMENT Ref. NO.- 08
REV:- 00 DATE :- 14.02.2022
NAME: Method Statement of Brick Bat Hardcore 

NDMMPL PROJECT :- DELHI 7 T

CONTRACTOR :- Society of Green Makers (P) Ltd. CMC :- CBRE South Asia CLIENT :- NDMMPL

he next day will be done the gap filling with the binding material (cement mortar) ratio 1:4.

 Followed by curing to be done for 3 days.

 Then the top surface will be given for screed concrete works.